PSA Self-Adhesive Nylon Hook and Loop Tape
PSA Self-Adhesive Nylon Hook and Loop Tape Thumb

PSA Self-Adhesive Nylon Hook and Loop Tape

Reference price US$0.05 – 1.20 / m FOB Xiamen · varies with width and order quantity
  • Model No: vc-325

  • Specifications

    Width : 10-150 mm, slit to order (+/-0.5 mm)
    Material : 100% Nylon
    Colour : Natural / made to order
    Minimum order : 500 m (stock colour) / 3,000 m (dyed)
    Sample : 7 days, cut to width
    Production : 2-3 weeks after sample approval
    Certification : SGS / Oeko-Tex / ISO 9001; REACH and RoHS declarations
    Packing : Polybag, export carton, palletised for LCL
    Port : EXW Xiamen, FOB or CIF
    Payment : T/T 30% deposit, balance against copy of B/L
    Slitting tolerance : ±0.5 mm
  • Inquiry now

Detailed description

There is no single grade of hook and loop, only grades matched to a job. The material, the width and the put-up below are the three variables worth settling before the first order, because changing any of them later re-opens the price.

What the buyer is choosing

Colour is a specification, not a preference. Dyed lots are matched to a retained standard under D65 light, and a black that matches in an office can read green in daylight. If the colour is customer-facing, approve a physical swatch and keep it, because a photograph is not a standard.

The material question

The fibre is nylon (polyamide). It takes dye deeply, which is why the colour range is wide and why the colour holds through washing at 40 degrees. Its weakness is moisture regain: a nylon roll absorbs water in transit, measures wide on arrival and settles back over about a week, so allow for it in incoming inspection rather than rejecting the lot.

This one carries a pressure-sensitive backing, so the substrate decides the result more than the tape does: powder coat and acrylic hold, polypropylene and polyethylene have too little surface energy and will let go under load.

How it is quoted

Minimum order is 500 m in a stock colour and 3,000 m for a custom dye run. The dye minimum is a machine load, not a policy: below it the lot cannot be dyed evenly, and a split lot reads as two colours under D65.

What ships with the goods

Peel and width are measured on the production lot, not on a sample kept from an earlier run. If your incoming inspection uses a different pull speed or dwell time, tell us and we will match it so the two numbers can be compared.

Checking it on arrival

Open one carton from the middle of the pallet, not the top. Condensation and compression both show up in the middle of a stack, and the top carton is the one that was packed with the most care.

Send the grade, width and colour with the annual volume and the quote comes back against a real construction rather than a catalogue range.

Send us your question about this product